Part NO. mb 207 front305200.00 Paint Electrophoretic Paint
Spec. 60*14 Model Mitsubishi Front
Material SUP9 MOQ 50 SETS
Free Arch 182±6mm  Development Length 1300
Weight 15.54KG Total PCS 2 PCS
Port SHANGHAI/XIAMEN/OTHERS Payment T/T,L/C,D/P
Deliver Time 15-30 days Warranty 12 months


Product Detail

Product Tags

Structure Chart

bbb
Parabolic Front Leaf Spring for Scania Truck Suspension

Technology Advantage

mb 207 front305200.00,According to the assembly sequence: the first piece, with a length of 1300, is rolled at both ends, and both ends are processed into lug shape, and two rubber composite bushings are assembled. The second piece, with a length of 1300, is rolled at both ends, and both ends are processed into lug shape, and noise reduction holes are punched at both ends; After assembling the assembly leaf spring, the arc height of the assembly is 182 ± 6mm. Two noise reduction plates are installed at the second punching noise reduction hole to reduce the noise generated during the action of the leaf spring. Clamps and central holes are installed at both ends of the assembly leaf spring φ 10.5. The product is applicable to Mitsubishi automobile series, and the main market is in Southeast Asia

The advantages of our factory

ITEM

SIZE

KG

1

MK334651-FA-3L

70*12/18

30.4

2

MK310031-FA

70*10

25.4

3

MK473242/3

89*12/22

77.2

4

MK 382877R

90*30

120.3

5

MK 305347F

90*22

82.3

6

MK315899F1

90*9/18

84.2

7

MK432506R

70*12/13/18

26.8

8

MK471936FA

70*8/10/11

29.9

9

MK301802R

90*22

92.9

10

MK317986F-01-010

80*14/20/21

61.3

11

MK301807H

90*12/14

47

12

MK470171-010

70*8/11

31

13

MK470174

70*6/10/11/12/14

58.6

14

MK383732-FA

70*11

27.6

15

DRS-MK470174

70*6/11/12

22.1

16

TW MK-301807H ASSY

90*14

42.3

17

MK3552 RA

90*20

154.9

We are very strict about quality

1) Raw matrail .
Thickness less than 20mm. We use material SUP9
Thickness from 20-30mm.We use material 50CRVA
Thickness more than 30mm. We use material 51CRV4
Thickness more than 50mm. We choose 52CrMoV4 as the raw material
2) Quchenging Process
We strickly controled the steel temeprure around 800 degree.
we swing the spring in the qenching oil among 10 seconds according to the spring thickness.
3)Shot Peening.
Each assmembing spring set under stress peening .
Fatigue test can reach over 150000 cycus
4) Electrophoretic paint
Each item use electrophoretic paint
Salt spray testing reach 500hours

Production Process

Bogie Spring (4)

Our Quality

  • Our Quality (1)
  • Our Quality (2)
  • Our Quality (3)
  • Our Quality (4)
  • Our Quality (5)
  • Our Quality (6)
  • Production Process (1)
  • Production Process (1)
  • Production Process (2)
  • Production Process (3)
  • Production Process (4)
  • Production Process (5)
  • Production Process (6)
  • Production Process (7)
  • Production Process (8)

  • Previous:
  • Next:

  • Write your message here and send it to us